[1]董贺新,郭士岭,王静..高岭土原位合成ZSM-5中活性铝含量分析及影响[J].郑州大学学报(工学版),2013,34(04):103-106.[doi:10.3969/j.issn.1671-6833.2013.04.024]
Dong He-xin,Guo Shi-ling,Wang Jing.Content Analysis of Activated Aluminum and its Influence Basedon In-situ Synthesis of ZSM - 5 on Kaolin[J].Journal of Zhengzhou University (Engineering Science),2013,34(04):103-106.[doi:10.3969/j.issn.1671-6833.2013.04.024]
点击复制
高岭土原位合成ZSM-5中活性铝含量分析及影响()
《郑州大学学报(工学版)》[ISSN:1671-6833/CN:41-1339/T]
- 卷:
-
34
- 期数:
-
2013年04期
- 页码:
-
103-106
- 栏目:
-
- 出版日期:
-
2013-09-09
文章信息/Info
- Title:
-
Content Analysis of Activated Aluminum and its Influence Basedon In-situ Synthesis of ZSM - 5 on Kaolin
- 作者:
-
董贺新; 郭士岭; 王静.
-
郑州大学化工与能源学院,河南郑州,450001, 郑州大学化工与能源学院,河南郑州,450001, 郑州大学化工与能源学院,河南郑州,450001
- Author(s):
-
Dong He-xin ; Guo Shi-ling; Wang Jing
-
School of Chemical Engineering and Energy ,Zhengzhou University,Zhengzhou 450001,China
-
- 关键词:
-
高岭土; ZSM-5; 原位晶化; 活性氧化铝
- Keywords:
-
kaolin ZSM -5 ; in-situ crystallization ; activated aluminum
- 分类号:
-
TQ170.1,TQ426.95
- DOI:
-
10.3969/j.issn.1671-6833.2013.04.024
- 摘要:
-
采用EDTA容量法,以PAN作为指示剂,准确分析不同温度下焙烧高岭土中的活性铝含量,滴定终点颜色变化明显.并讨论了活性硅、活性铝含量对原位晶化合成ZSM-5型分子筛的影响.750℃焙烧高岭土、外加铝源的950℃焙烧高岭土都难以合成出ZSM-5型分子筛.以950℃焙烧高岭土为载体和唯一铝源,外加硅源,适当调节碱、硅、水加入量,在150℃,高硅铝比条件下得到杂晶少、结晶度较高的产品.通过此方法可区分高岭土中载体铝和用于合成的活性铝.原位晶化合成中硅铝配比以活性铝、活性硅含量计算较为合理.
- Abstract:
-
Taking PAN as indicator,a precise content analysis method of the activated aluminum which con-sists in calcined kaolin in the different temperature by the EDTA volumetric method is introduced in this pa-per. The color change of end-point is obvious. And the effect about content of activated aluminum based onin-situ crystallization synthesis of ZSM -5 is also discussed.ZSM -5 is difficult to be synthesized in situ crys-tallization in the kaolin calcined at 750 ℃ or at 950 ℃ added to the aluminum source.Crystallization productswith little impure crystal,high degree was synthesized under the following conditions: the kaolin calcined at950 ℃ as carrier and the only source of aluminum,adjunction of silicon source, appropriate regulation of al-kali,silicon and water content,synthesis temperature of 150 ℃. With this method,A distinction should bemade between the difference in kaolin carrier of aluminum and used for the synthesis of active aluminum. Andthis paper presents a general method that act Si ( activated silicon )-Al ( activated aluminum ) ratio as the ratioof synthetic zeolite in situ crystallization.
更新日期/Last Update:
1900-01-01